Why hollow a resin print
On a resin printer (SLA, MSLA or DLP), a solid part is solid resin all the way through. That is fine for small parts, but as models get bigger it becomes a problem:
- Cost. Resin costs several times more per kilogram than filament, and a solid figure uses all of it.
- Peel forces. Each layer is cured against the film of the vat and pulled off. A large solid cross-section sticks harder, which can tear the part from its supports or the build plate.
- Weight on the supports. A heavy solid part hanging upside down needs more and thicker supports, which leave more marks.
- Curing. UV light only cures the outer millimeters during post-curing. A thick solid part can keep uncured resin inside.
Hollowing leaves a shell of a chosen thickness and removes the inside. Drain holes let the liquid resin out and let air in, so there is no suction during printing. This guide uses Hollow STL on this site, which does both in the browser.
How much resin does hollowing save?
It depends on the size of the part much more than on any setting. We hollowed the sample part used on this site (46.5 × 48.4 × 22.9 mm, 13.66 cm³) with three wall thicknesses, and then the same part scaled two and three times, with a 2 mm wall:
Same part, different walls:
| Wall thickness | Resin saved | Of the original volume |
|---|---|---|
| 1.5 mm | 5.41 cm³ | 40% |
| 2 mm | 3.48 cm³ | 26% |
| 3 mm | 0.88 cm³ | 6% |
Same 2 mm wall, bigger part:
| Size | Volume | Resin saved | Of the original volume |
|---|---|---|---|
| 46 × 48 × 23 mm (×1) | 13.7 cm³ | 3.5 cm³ | 26% |
| 93 × 97 × 46 mm (×2) | 109.3 cm³ | 62.0 cm³ | 57% |
| 140 × 145 × 69 mm (×3) | 368.8 cm³ | 257.4 cm³ | 70% |
The pattern is geometry: the wall’s volume grows with the surface (the square of the size), while the total volume grows with the cube. At three times the size, the same 2 mm wall leaves 70% of the resin unused. On a small part, a thick wall leaves almost nothing to remove: at 3 mm, our 23 mm tall part is nearly all wall.
Rule of thumb: below about 30 mm in every direction, hollowing saves little and adds work. Above 60 to 80 mm, it is almost always worth it.
Choosing the wall thickness
- 1.5 mm: the minimum for small to medium figures in standard resin. Saves the most but is fragile, especially around drain holes and thin features.
- 2 to 2.5 mm: a good default for figures, busts and display pieces.
- 3 mm or more: large parts, parts that will be handled, sanded or drilled, and brittle resins.
- Tough and flexible resins can go thinner; very brittle “high detail” resins need more.
Thin features, such as fingers, swords, ears or tails, are usually thinner than twice the wall, so they stay solid after hollowing. That is correct: there is nothing to remove inside them.
Drain holes: where and how big
A hollow part without holes is a sealed balloon. During printing, every layer that closes the cavity creates suction against the vat film; afterwards, uncured resin stays trapped inside and can leak or crack the part months later as it slowly expands. Holes are not optional.
- At least two holes: one lets resin out while the other lets air in. One hole alone drains slowly and still creates suction.
- Near the build plate. On a part printed upright, holes in the lowest area let resin drain during the print and the wash. Hollow STL opens them in the flat base of the model; on a part with no flat base, open them yourself in your slicer.
- Size: 3 to 5 mm is typical. Under 2 mm, thick resin drains very slowly and holes clog.
- Hidden spots: under the base, behind a cloak, in the sole of a foot. They can be plugged after curing with a drop of resin and a short UV exposure.
Washing and curing a hollow part
- Drain with the holes facing down, before the wash, for a few minutes.
- Wash inside: shake the part in alcohol or the cleaning liquid so it flows through the cavity, or use a syringe through a hole.
- Dry completely, inside too. Alcohol trapped inside clouds the resin and can crack the shell during curing.
- Cure. UV reaches the inside only through the holes, so the inner surface stays softer. That is normal; what matters is that no liquid is left.
Hollowing in the slicer or before it?
Chitubox, Lychee and PrusaSlicer can hollow and add holes too. Hollowing the STL before slicing has two advantages: you get a file you can check, share or print anywhere, and you see the real volume and savings before committing. Hollow STL keeps the outer surface untouched and builds the inner wall from a voxel grid, so it handles complex sculpted models, and everything runs on your device without uploading the model.
Checklist
- Is the part big enough to benefit? Over about 60 mm, yes.
- Wall of 2 to 2.5 mm for figures; 3 mm for parts that will be handled.
- At least two drain holes of 3 to 5 mm, low on the part and hidden.
- Drain, wash inside, dry fully, then cure.